MSCL pipe, spigot and socket ends, cement lined, SIRIM certified to SPAN TS 21827
MSCL pipe (SIRIM, SPAN TS 21827) — dimensions and ratings
Nominal DN (mm)OD (mm)Min wall BS 534 (mm)Min wall SPAN TS (mm)Min concrete lining (mm)Bitumen wrap (mm)Weight BS 534 (kg/m)Weight SPAN TS (kg/m)Hydraulic test pressure (bar)
100114.33.63.6639.89.870
150168.33.63.66314.614.670
200219.14.04.010321.221.270
250273.04.04.010326.526.556
300323.94.04.010331.631.648
350355.64.54.513339.039.049
400406.44.54.513344.644.643
450457.05.05.013355.755.742
500508.05.05.013362.062.038
600610.06.36.313393.893.840
700711.06.36.3193109.5109.534
800813.07.17.1193141.1141.134
900914.07.18.0193159.0178.734
10001016.07.18.0193177.0198.930
12001219.08.010.0193239.0298.132
14001422.08.810.0253307.0348.227
16001626.010.011.0253399.0438.126
18001829.011.012.5253493.0559.926
20002032.012.514.2253623.0706.627
  • SIRIM-certified MSCL pipe to SPAN TS 21827, spigot & socket ends, bitumen or painted (green) finish. Schedule as published by the manufacturer (selected sizes shown; the full source table extends to DN2700).
  • Hydraulic test pressure column applies to steel 430 yield class, per the source table.
  • Where BS 534 and SPAN TS values differ (DN900 and above), order to the standard your tender cites.

Data source: data/product-specs/mscl-pipe-span-ts-21827.md (transcribed from manufacturer data; verify against latest catalogue revision before fabrication).

About this schedule

These figures are transcribed from the MSCL pipe manufacturer’s schedule published on our product page for SIRIM-certified MSCL pipe to SPAN TS 21827. Selected sizes are shown above; the source schedule extends to DN2700 — request the full schedule for sizes not listed.

How engineers use this table:

  • Weights for logistics. Use the weight column matching your cited standard for delivery planning and trench/shoring design. At DN2000 the difference between standards is over 80 kg per metre — it adds up over a kilometre.
  • Lining and wrap for inspection. The concrete lining (6–25 mm) and bitumen wrap (3 mm) minimums are what inspection measures against. Quote them in your material submittal.
  • Test pressure for commissioning. The hydraulic test pressure figures (steel 430 class) feed the pressure test procedure — verify against the design consultant’s requirement for your class of pipe.

For the material-selection debate, see MSCL vs ductile iron for water reticulation.

Fabricated fittings

The matching MSCL fitting range — 45° and 90° bends, tees, and tapers, in bitumen or painted finish, plain ends, SPAN TS, SIRIM — is stocked to match these barrels. See MSCL pipes and MSCL fittings for stock or send your fabrication drawings for quotation.